PROTMAX (CECRI) ANTCORROSIVE TREATMENT PROCESS |
|
|
PERFORMANCE DATA |
|
|
Tests Spec: ASTM A775/775M-84 |
|
| Chemical Resistance Test - 45 Days | |
|
3M Cacl2 |
No softening, swelling, blistering or cracking was observed at the end of 45 days. |
| 3M NaOH | |
| Saturated Ca(OH)2 | |
| Distilled Water | |
|
2V impressed voltage test (Accelerated Corrosion) |
|
|
Medium: 7% NaCl Voltage Impressed: 2V Duration-1 hour |
At the end of 1 hour, no dissolution, no disbondment of the coating was observed |
|
Technical Data |
|
| Salt Spray test | 2000 Hours |
| Tolerable limit for chlorides | 10000 ppm |
| Salt fog test | > 2000 Hours |
| Alternate wetting & drying under load | >450 days |
| Bond Strength | meets IS:456 as per clause No.0.2.2.11 and 44 1.2 -Tested as per IS:2770(Part1) |
| Hardness using pencil hardness | 5H to 7H |
| Thickness of coating | 200 to 300 microns |
| Note: The above tests have been conducted by CECRI (Central Electro Chemical Research Institute) and results published in CECRI literatures. | |